What Problems Should be Paid Attention to before Baking the Tundish?
(1) Within 1 to 2 hours before the pouring of the tundish, boil quickly to 1000~1100 °C, preferably cast steel immediately. (2) For a long time of baking, the carbon…
Read moreLoading
(1) Within 1 to 2 hours before the pouring of the tundish, boil quickly to 1000~1100 °C, preferably cast steel immediately. (2) For a long time of baking, the carbon…
Read moreEvery day, we have time to share the orders. At this time, the colleagues who have made the order will share their own history. This time is the sharing of…
Read more(1) Brick selection. Any defective bricks that exceed the standard requirements such as cracks, blisters, fire smashes, ribs, corners, distortions, uneven end faces, missing sub-ports, looseness, and excessive dimensional tolerances…
Read moreThere are two methods on the masonry of refractory bricks in the mold casting bottom plate. (1) Dry laying method. The brick interface does not smear the mud in the…
Read moreThe turnkey project of circulating fluidized bed gasifier with a total of more than 4,000 tons of refractory materials undertaken by the RS Group, has been fully started. RS Group…
Read moreFirst, the same horizontal plane (the brick and the bottom plate are on the same level), Second, thick (the sand at the bottom of the tank is densely packed), Third,…
Read moreRongsheng Refractory Factory provides various refractory bricks and thermal insulation materials for the iron and steel smelting industry. Linzhou Heavy Machinery Lingang Iron & Steel Co., Ltd. is mainly engaged…
Read more